My previously mentioned crystals came through for me and gave a nice structure with a decent R factor. 5.9, which is fair, for small molecule work the goal is really less than 5, but 5.9 is fine with me. I might try to solve the structure myself just to see if I can't get it down a little farther. I'm guessing that the staff crystallographer just punched the "solve" button and went with the computer answer, so I could probably shave a few more thenths off the R factor with some careful work. Don't hold your breath though.
The next success dates back to something I've been trying to do since the first week I arrived here. In the very first post I made I referred to a compound I was attempting to sublime in an effort to purify it. Purification of this product has been an absolute pain in the tuckus. Crystallization (via layering, slow cooling, slow evaporation, crashing) sublimation, chromatography, and chemically protecting/deprotecting have not worked at all. What did work was just decreasing the amount of material that I was trying to make at once. There's no reasonable explanation for why this would work, but its tough for me to worry too much about something that worked out well for me. The NMR shows better than 99% purity. Awesome.
So if good things come in threes that means I should have something else good coming my way. Today I'll be working on the Ir recycling by flipping the switch on the muffle furnace and letting that sucker plug away all day. I've been having trouble determining what the right temperature is that the iridium oxide needs to be at in order to decompose to the metallic iridium. I haven't really found any reliable numbers for this, but Wikipedia suggests that 1100 C is just about where I need to be. Please note that Wikipedia is not a credible source. Not that's its wrong, but its like writing a book report and citing Cliff's Notes. The muffle furnace I'll be using maxes out at 1100 C, but we'll see just how far I can push it. 1200 C would be nice, just to make sure that the job gets done.
August 13, 2007
August 9, 2007
salespeople
A short commentary on salespeople.
From time to time in the course of working in a research lab it may become necessary to order some expensive pieces of equipment. I don't relish the experience of talking to sales people but for the most part this is mitigated by the fact that they want to sell stuff to you. Something about commission, I'm sure. What baffles me is that when I need specific information from them, and they get all cagey, like all of a sudden they don't want this sale to continue if it means looking something up or doing a little math. Let me clue in all of the salespeople who I know must read this blog. (*cough*) Price is an object to a graduate student only to a certain extent, after that, the most important things in closing a deal is expediency and minimization of hassle. I don't work in the Purchasing and Acquisions office, I'm a grad student. My patience for paperwork is very thin and if there are two vendors offering nearly the same services, I will take the one that is fast and helps me through my paperwork over the one which is 10% cheaper. Valuable information for anyone trying to sell something to a chemist in my position.
From time to time in the course of working in a research lab it may become necessary to order some expensive pieces of equipment. I don't relish the experience of talking to sales people but for the most part this is mitigated by the fact that they want to sell stuff to you. Something about commission, I'm sure. What baffles me is that when I need specific information from them, and they get all cagey, like all of a sudden they don't want this sale to continue if it means looking something up or doing a little math. Let me clue in all of the salespeople who I know must read this blog. (*cough*) Price is an object to a graduate student only to a certain extent, after that, the most important things in closing a deal is expediency and minimization of hassle. I don't work in the Purchasing and Acquisions office, I'm a grad student. My patience for paperwork is very thin and if there are two vendors offering nearly the same services, I will take the one that is fast and helps me through my paperwork over the one which is 10% cheaper. Valuable information for anyone trying to sell something to a chemist in my position.
August 8, 2007
guarded optimism
The crystals I sent the X-ray lab seem to have held up in the mounting oil and diffracted well enough. The strong scattering (shown in the picture) and unit cell dimensions indicate some sort of monomer with one heavy atom (the metal atom) per unit cell. I don't have the solved structure in hand yet, but I'm ready to declare victory as far as getting a quality crystal. I've seen better, these were pale orange needles. Not too shabby though.
X-ray quality crystals were grown from a standing cooled solution in heptane over several weeks at a temperature of -35 C.
X-ray quality crystals were grown from a standing cooled solution in heptane over several weeks at a temperature of -35 C.
August 7, 2007
a break from recycling, and some crystals
Finally, some good news. But first an update on the frustrations of the Ir recycle project. The setup for chlorination was tested, but due to operator error, some adjustments may have to be made. I'm suspicious that the dedicated gas regulator for the Cl2 gas tank is corroded to the point of uselessness, however this is no excuse for ineptitude, at least not yet. In better news, I have located a muffle furnace, so perhaps this is an end to the current destruction of crucibles from around the department. More on that later.
CRYSTALS! A vial left in the freezer has yielded some needly orange crystals. Perhaps not the best for crystallographic analysis, but the crystallographer here thought they would be just fine. Currently I'm awaiting time on the diffractometer, so we'll wait before I declare total success. I'm still counting it as a triumph to get crystals at all, though.
CRYSTALS! A vial left in the freezer has yielded some needly orange crystals. Perhaps not the best for crystallographic analysis, but the crystallographer here thought they would be just fine. Currently I'm awaiting time on the diffractometer, so we'll wait before I declare total success. I'm still counting it as a triumph to get crystals at all, though.
August 1, 2007
Ir recycling step 5.1
The thermal shock on the crucibles has proved to be too much. Recall that the Meker burner did not generate enough heat to reduce the ash mixture to elemental material and salts, but it did come close. The solution then, or so I thought, was to use more Meker burners set up in a tripodal fasion. This (I patted myself on the back a few times for this) would allow greater control over slow heating as well as provide more actual area on on the crucible which was being heated so as to not develop "hot spots" on the crucible itself (slow heating is ineffective if the thermal shock is due to one area of the crucible expanding while another cool area does not.)
I set up (painstakingly) a couple of stands with Meker burners perfectly in place for the tripod along with the crucible at the optimal height and then started up all the Meker burners at the lowest possible gas flow. I increased the gas flow slowly on each of the burners over the course of about twenty mintues, carefully monitoring all of the surroundings to make sure they were not overheating.
Long story short the heat load was too much for the dry powder fire extinguisher which comes standard on all of the hoods in the lab. The heat triggered nozzle fired fine yellowish powder all over myself, the setup I was so proud of and half of the lab. A picture (of course) of the misery will follow shortly after I get it off of Krista's camera.
I set up (painstakingly) a couple of stands with Meker burners perfectly in place for the tripod along with the crucible at the optimal height and then started up all the Meker burners at the lowest possible gas flow. I increased the gas flow slowly on each of the burners over the course of about twenty mintues, carefully monitoring all of the surroundings to make sure they were not overheating.
Long story short the heat load was too much for the dry powder fire extinguisher which comes standard on all of the hoods in the lab. The heat triggered nozzle fired fine yellowish powder all over myself, the setup I was so proud of and half of the lab. A picture (of course) of the misery will follow shortly after I get it off of Krista's camera.
July 10, 2007
Ir recycling step 5
This is a note of contention as to whether or not this step is necessary. Professor Heller suggested that the black Ir/ash was good enough to carry on, while I thought this step would yield better results. As such, I'll do some of the batch both ways and see if the result is the same.
I've used a glassblowing torch in order mix some O2 in with the natural gas. This increases the temperature of the flame considerably, enough so that the bottom of the crucible glows like a light bulb. After a fews tens of minutes of heating, the black Ir/ash has melted into a glowing red lava-like goo. There were two separate layers evident, what I can only guess is metalic iridium made up the glowing red material in the bottom of the crucible, covered by a clearish liquid layer which I'm guessing is molten salts. This step gave off some pretty intense radiant heat, making me wonder if the fire extinguishers in the top of the hood would be triggered, happily this did not occur.

Several attempts were made to get this process to work correctly. I was successful once, shown in the picture, but subsequent attempts led to the crucibles breaking due to thermal shock and uneven heating. I tried to remedy this by using a Meker burner on full blast for hours, but the temperatures achieved was not enough to convert the ash to salts and the (presumably) iridium oxides to metallic iridium. I tried to spread the flame of the glass blowing torch out by loosely affixing the Meker burner grating to the top of the torch, but the O2 content was too high in the cavity in between, leading to a lot of backfiring and me almost crapping my pants. Clearly, a safe, more controlled heating method is needed, either by furnace or adapting the current setup to prevent thermal shock to the crucible and promote even heating. More on this soon....
I've used a glassblowing torch in order mix some O2 in with the natural gas. This increases the temperature of the flame considerably, enough so that the bottom of the crucible glows like a light bulb. After a fews tens of minutes of heating, the black Ir/ash has melted into a glowing red lava-like goo. There were two separate layers evident, what I can only guess is metalic iridium made up the glowing red material in the bottom of the crucible, covered by a clearish liquid layer which I'm guessing is molten salts. This step gave off some pretty intense radiant heat, making me wonder if the fire extinguishers in the top of the hood would be triggered, happily this did not occur.

Several attempts were made to get this process to work correctly. I was successful once, shown in the picture, but subsequent attempts led to the crucibles breaking due to thermal shock and uneven heating. I tried to remedy this by using a Meker burner on full blast for hours, but the temperatures achieved was not enough to convert the ash to salts and the (presumably) iridium oxides to metallic iridium. I tried to spread the flame of the glass blowing torch out by loosely affixing the Meker burner grating to the top of the torch, but the O2 content was too high in the cavity in between, leading to a lot of backfiring and me almost crapping my pants. Clearly, a safe, more controlled heating method is needed, either by furnace or adapting the current setup to prevent thermal shock to the crucible and promote even heating. More on this soon....
July 9, 2007
Ir recycling step 4
The crucible of concentrated nastiness has removed most of the volatiles, which will prevent a huge flame ball from forming in this step. Here, we are simply heating off any of the volatile salts and burning solid organics down to ash. The iridium/ash may be good enough to carry on, however, the recycling will be much easier after heating to higher temperatures. The setup is shown below: a crucible with the iridium residues being fired by a Meker burner with the air mixer on low, gas on low. Lots of smoke (fairly toxic) is given off in this step. Although the picture is taken with the sash up, it was down for the duration of the burn-off, save for the picture.
July 3, 2007
Ir recycling step 3
Many of the higher boiling solvents and other nasties (mineral acids, oils, phospines, etc.) are still present and the waste residue currently has the consistency of chunky fondue. Unfortunately the smell doesn't resemble fondue in the least. Many of the bad smelling, high boiling residues left are removed by extensive heating in a crucible to 300 - 350 C using a heating mantle and sand bath. This was also a good time to throw in the tissue papers I used to clean up a few spills. No worries, as all of the organics are being decomposed in the hot acid and will be fired off in the next step.
Ir recycling step 2
The next step is to strip all of the volatile materials from the waste, employing a Rotovap. This is merely a contraption which heats the solvent in one pot while cooling the vapors so that they drip into another pot (the solvent trap.) This step happened mostly without incident, save but one batch of waste which was not properly neutralized. Of course, if you take dilute acid and strip the solvents off, what you end up with is concentrated acid. This hazard is inherent, since most of the volatiles are benign, anything which is particularly nasty is going to be concentrated and become nastier. As my labmate says, usually to make himself feel better while pouring waste down the drain with the water on, "The solution to pollution is dilution!" I have discovered the opposite is also true "If you want to make nasty waste even worse, concentrate it!" Its not as catchy, but equally relevant to the task at hand.
This nastiness will all be remedied in the next step.
This nastiness will all be remedied in the next step.
Ir recycling step 1
The first thing to do is collect the waste. As you can see in the photo, there is a good bit of it from the various labs in the department. Some of it has been evaporated already, so its pretty dense. Most of it, however, is a lot of solvent for not a lot of metal. This picture shows the bulk of what I collected initially. In the present form of whatever it was collected in I would estimate the volume to be 4 to 5 liters.
June 23, 2007
precious metal recycling
I just had one of the first years make a boat load of the starting material he and I will both be using for our projects over the summer. He scaled up enough to use all of the remaining iridium (Ir) which was in the department, meaning that if we ever need to make this material again, we will have to buy more Ir. Iridium is pretty expensive, at the current market prices it costs just a tad under the price of gold, but that doesn't reflect the actual obtainable price because there are a lot more people out in the world dealing gold than iridium. Strem will sell the hexachloroiridate salt for 50$ per gram.
I've embarked upon recycling the iridium waste in the division for both practical reasons as well as pure interest in the brute force methods required to recover iridium residues back into usable materials. The procedure is basically this:
1. collect the waste
2. evaporate the low boiling solvents (<100 degrees C with partial vacuum)
3. evaporate the high boiling materials (heating mantle at about 300 degrees C)
4. fire the residues to ash (Bunsen burner with the air mixer open pretty far)
5. crush the ash and fire to redness (Meker burner with the air mixer open as far as possible.)
That gets to the raw metal, which is where I'll leave it for now. I think this whole process is pretty interesting, so I'll keep the individual steps updated on the blog. The method isn't proprietary and can be found in "The Journal of Less Common Metals", a tome of which I have never seen nor heard of until I starting this process.
I've embarked upon recycling the iridium waste in the division for both practical reasons as well as pure interest in the brute force methods required to recover iridium residues back into usable materials. The procedure is basically this:
1. collect the waste
2. evaporate the low boiling solvents (<100 degrees C with partial vacuum)
3. evaporate the high boiling materials (heating mantle at about 300 degrees C)
4. fire the residues to ash (Bunsen burner with the air mixer open pretty far)
5. crush the ash and fire to redness (Meker burner with the air mixer open as far as possible.)
That gets to the raw metal, which is where I'll leave it for now. I think this whole process is pretty interesting, so I'll keep the individual steps updated on the blog. The method isn't proprietary and can be found in "The Journal of Less Common Metals", a tome of which I have never seen nor heard of until I starting this process.
June 21, 2007
glassblowing and joint sweating
Glassblowing is necessary from time to time in order to fix something you just broke, make a piece of glassware which you need right now, and so forth. Our glassblower arrives biweekly, so if you want something done by him it usually takes a long time, which could be remedied if the physics shop (which houses the glassworks) would just let us use the damn annealing oven.
We needed a piece of tube with a 3/8th inch outer diameter attached to a length of 1 inch tube with a standard taper 24/40 joint. This is nothing more than a tube, attaching one end straight on to the other. I tried for some time to make the first attachment to no avail. I could get as far as blowing out the end of the tube to make an even edge, but I was completely inept at attaching the two pieces. After several poor attempts Professor Heller learned of what I was doing, and although he thought it was admirable, was quick to point out exactly where I was failing.
I was missing a swivel joint used so that you could blow into a tube connected to the end of the glass and spin it at the same time. I distinctly remember that the last time I watched Heller connect two tubes together he did it without the aid of the swivel joint and did just fine. Apparently he was just showing off.
Hand annealing is another issue entirely, as Heller doesn't seem to have the patience to do it properly and as stated earlier, the physics shop doesn't let us use the oven. So even though the piece has been made it still can't be used because its too brittle in the present form.
On a similar note, sweating a joint in copper tubing was also on the day's chore list. I've seen my father and grandfather do it several times. The made it look ridiculously easy, just polish, flux, and sweat. This is a lot easier if you remember that you need the flux, which I forgot about on the first several attempts. I read on line that if you were doing this on household plumbing the best way to keep the water out is to jam a wad of white bread into the pipe before you sweat the joint, then just flush it out after you're done.
Curiously enough chemical stores does not stock white bread.
We needed a piece of tube with a 3/8th inch outer diameter attached to a length of 1 inch tube with a standard taper 24/40 joint. This is nothing more than a tube, attaching one end straight on to the other. I tried for some time to make the first attachment to no avail. I could get as far as blowing out the end of the tube to make an even edge, but I was completely inept at attaching the two pieces. After several poor attempts Professor Heller learned of what I was doing, and although he thought it was admirable, was quick to point out exactly where I was failing.
I was missing a swivel joint used so that you could blow into a tube connected to the end of the glass and spin it at the same time. I distinctly remember that the last time I watched Heller connect two tubes together he did it without the aid of the swivel joint and did just fine. Apparently he was just showing off.
Hand annealing is another issue entirely, as Heller doesn't seem to have the patience to do it properly and as stated earlier, the physics shop doesn't let us use the oven. So even though the piece has been made it still can't be used because its too brittle in the present form.
On a similar note, sweating a joint in copper tubing was also on the day's chore list. I've seen my father and grandfather do it several times. The made it look ridiculously easy, just polish, flux, and sweat. This is a lot easier if you remember that you need the flux, which I forgot about on the first several attempts. I read on line that if you were doing this on household plumbing the best way to keep the water out is to jam a wad of white bread into the pipe before you sweat the joint, then just flush it out after you're done.
Curiously enough chemical stores does not stock white bread.